EXTRA WHITE CASTING GRAINTIPS FOR USING EXTRA WHITE CASTING GRAIN / ULTRA WHITE CASTING GRAIN
Annealing: Heat in an
oven set to 1350-1400º F for 20 minutes, depending on the size of the
castings. Quench immediately for 2-4 mins. Do not allow to air cool.
Under certain conditions, all nickel-white gold alloys are susceptible
to stress corrosion. 14K EXTRA WHITE (14WXCG) Liquidus 1730º F 18K EXTRA WHITE (18WXCG) Liquidus 1702º F Cast Temp. 150º F - 225º F above Liquidus Temperature Platinum casting grain in 90/10 and platinum casting grain in 95/5 round out the white casting grain picture on the higher end. 14K
CASTING GRAIN IS ALSO KNOWN AS: Tips For Using Extra White / Ultra White Casting Grain G&S Metals mission is to provide quality products, friendly, personal and helpful service at competitive prices and in a timely fashion. Orders are shipped the same day and price in based on the London PM fix. Our integrity and expertise in refining has generated customer confidence and support for over 50 years.
All
Extra White Casting Grain, Jewelry Findings
|
||
|
G&S Metals, Inc. |
|||